Annealed wire is a soft iron wire made of low carbon steel cold drawing, heating, constant temperature, heat preservation and other processes. The composition of iron wire varies according to its use. It contains iron, cobalt, nickel, copper, carbon, zinc, and other elements. The hot metal billet rolled into 6.5mm thick steel bar is the wire rod, and then put it into the wire drawing device into a different diameter of the line, and gradually reduce the aperture of the wire tray, cooling, annealing, plating and other processing technology made of various specifications of iron wire.
Therefore, the rust of galvanized black iron wire has a great relationship with storage. At the same time, after rust, it should also be reasonable for post-treatment to avoid affecting its use effect. Of course, when the black iron wire is galvanized, the thickness of the galvanized layer should be ensured, so that the possibility of rust can be reduced. Speaking of galvanized iron wire, perhaps many people think it is relatively rare, in fact, it is not.
In our daily life, we are certainly familiar with the construction of power grid. Choosing such special barbed rope can improve the safety factor of the entire power grid during construction. In fact, after the construction of the power grid does not need to be energized, the only security measures can play the equipment is these galvanized barbed rope, in the choice of time is certainly to choose some of their own needs, and the quality of the product of reliable materials.
Good galvanized wire, plating thickness of 3- 4 mm, zinc adhesion should be less than 460 grams/m, that is, the average thickness of zinc layer is not less than 65 microns. When the thickness of plated parts is greater than 4 mm, the zinc adhesion should not be less than 610 g/m, that is, the average thickness of zinc layer should not be less than 86 microns. Standard galvanized wire coating must be uniform, galvanized layer basically uniform with copper sulfate solution test etching five times no dew iron. For standard galvanized wire coating adhesion requirements, the zinc layer of plated parts should be firmly combined with the basic metal and have enough adhesion strength, after hammer test does not fall off, not convex.
Therefore, the rust of galvanized black iron wire has a great relationship with storage. At the same time, after rust, it should also be reasonable for post-treatment to avoid affecting its use effect. Of course, when the black iron wire is galvanized, the thickness of the galvanized layer should be ensured, so that the possibility of rust can be reduced. Speaking of galvanized iron wire, perhaps many people think it is relatively rare, in fact, it is not.
Corrosion usually metal corrosion has three types: physical, chemical corrosion and electrochemical corrosion, and corrosion depends on the chemistry of the metal itself and the organizational structure, still have relationship with the surrounding medium, such as wet environment than dry environment is easy to rust, more less than the impurities of impurities is easy corrosion, high temperature conditions than under the condition of low temperature corrosion, etc. After knowing these, we can effectively prevent the corrosion of the dip plastic six side wire mesh, prolong the service life of the product.
In reinforced concrete structure, the crack width of cold wire drawing is smaller than that of circular steel bar or even that of hot rolled thread bar. So cold wire drawing is more popular in the construction industry. The material for cold drawing is made of steel bars and can be simply explained how it is made, that is, its production process is simple. It’s based on steel bars, which are constantly stretched evenly, stretching the bars into something very thin, like wire drawing, without plasticity.
There is no adhesion test of powder spraying or fluorocarbon spraying on packaged galvanized wire, but there are two points for reference: first, in sealed or air-free environment, non-metallic volatiles can corrode zinc coating; Second, zinc at higher than 230 degrees (c) will cause the matrix metal brittle. And powder spraying and fluorocarbon spraying are to be baked at a higher temperature and in a sealed environment, causing rapid corrosion of zinc, resulting in loose corrosion film resulting in coating adhesion decline, and even lead to (matrix) steel wire brittle situation may exist.
The price of galvanized iron wire performance is the key to win, galvanized wire only with good performance, in order to win the market, in order to obtain customer praise. In galvanized wire, the main function of carbon in increasing hardness, less is less easy to rust, the main function of chromium is acid and alkali resistance; Nickel’s main function is high temperature resistance, acid and alkali resistance and conductive use; The main function of iron is magnetic conductivity; The main functions of titanium are low density, high hardness and strong corrosion resistance. The main function of copper is magnetic and electrical conductivity. Different chemical components have different functions, which together form the characteristics of galvanized wire.